I know I have seen it here before, but I can’t seem to find it now.  Which is better as far as the internals go?  304 Stainless Steel and Heat Treated Inconel 718 or Chrome Moly Steel.  I hope the first one is the better of the two, because I just ordered the YHM Phantom SS today.

Thanks,
D
12/3/2008 7:15:53 PM EDT
[#1]
Quoted:
304 Stainless Steel and Heat Treated Inconel 718



this

12/4/2008 4:13:39 AM EDT
[#2]
Quoted:
Quoted:
304 Stainless Steel and Heat Treated Inconel 718



this



Thanks for the help, Does anyone make a 7.62 with these internals?

D
12/4/2008 4:28:45 AM EDT
[#3]
Quoted:
Quoted:
Quoted:
304 Stainless Steel and Heat Treated Inconel 718



this



Thanks for the help, Does anyone make a 7.62 with these internals?

D



AAC uses 316 stainless and Inconel 716
316 is supposed to be better than 304... but Im not a steel guy.
12/4/2008 7:21:26 AM EDT
[#4]
Quoted:
Quoted:
Quoted:
304 Stainless Steel and Heat Treated Inconel 718



this



Thanks for the help, Does anyone make a 7.62 with these internals?

D



SAS (Supressed Armament Systems) in Elkhart, IN. will do the whole stack out of Incon as an option........